What did you print today?

This was one of my sub 1 gram prints that ended up being extremely useful for cheaper calipers.
My brother spent $200 on a set of Mituyo Calipers and the wheel is SMOOTH and does not wiggle.
Cheap calipers have a really shitty loose wheel, so I made a C-clip spacer to wedge it on the axle and it makes a cheap set of calipers feel much smoother to use.

Since it was on the caliper itself, I had to eyeball the measurements. On the first draft print, it snapped in place and it won't come out. I also made it purely within Prusa Slicer, so I couldn't even save it as an STL since I used a Cylinder with a "Negative Volume modifier" Cylinder in the middle, thus making it non-exportable (why can't I export a model with negative cut outs from my Slicer as an STL file?). At the time, I didn't know I could just export the project as a .3mf file :(
1793745856475.png




I'll try to print one out again today.
 
I've been using AI to help me generate DXF files so I can have a baseline to work from. I know Printables / MakerWorld / Thingiverse, etc are full of 75mm VESA mount models, but I just want one that is fixed that hangs on two thumbtacks. I really need to print out a peg board and install it on my wall.
This tablet is very light weight and it runs on an ARM processor so its very power efficient, and it takes a standard 12 volt input.

I know I could probably have asked Claude to just generate this much quicker, but I still like modeling manually in Fusion 360. Although this simple model still took me a few hours to finish cause I haven't used Fusion 360 in a while. I made it at a fixed 8 degree angle and 2.5 degrees upwards. A ball joint model could do the job, but I needed something that was low profile and flatter against the wall. I don't intend on changing the angle at all.

1793762004842.png


The thumbtack keyholes are hollow within the models, so I just bridged internally. There are two "V" cut outs to allow some ventilation for heat, even though this is an ARM processor that barely gets warm.
1793762148929.png


1793762159133.png


Printed with Aliexpress Black PETG. The biggest drawback with PETG and stronger filaments is the print speed limitation. 80mm/s is painfully slow.
 
Printed with Aliexpress Black PETG. The biggest drawback with PETG and stronger filaments is the print speed limitation. 80mm/s is painfully slow.
I realize I say this as someone with a professed limitation with PETG but I used to think this. My H2D prints 200mm/s and faster with PETG HF and non-HF variants... I thought the profile was insane but I tried it and sure enough it lays down very hot and comes out very strong. Even some PETG I know was made before high flow PETG was a thing prints just fine at those speeds...
 
Oh, I need one of those.

BTW I got one off Amazon, brand name is Esydon, that doesn't drain like that.
Funny enough, that's the exact brand I have, and it's the one with the problem lol. Maybe a slightly different make, or defect, or who knows at this point
 
I realize I say this as someone with a professed limitation with PETG but I used to think this. My H2D prints 200mm/s and faster with PETG HF and non-HF variants... I thought the profile was insane but I tried it and sure enough it lays down very hot and comes out very strong. Even some PETG I know was made before high flow PETG was a thing prints just fine at those speeds...
I might have to experiment and research about printing PETG faster with NO cooling. I know if you cool PETG "just to make a print quick", it will be SUPER brittle. Right now I have my PETG cooling enabled at all times, but only at 15% to 20% fan speed. I also have an enclosure, and I think a heat stable environment definitely helps.

One person told me that you can print PETG fast, but instead of cooling it, you blow heat at the print (through a remote CPAP hose).
 
Last edited:
One person told me that you can print PETG fast, but instead of cooling it,
On my Sovol, I have PETG set to print first layer speed of 120, with infill at 150. Other layers have inner walls and sparse infill as high as 230mm/s and I haven't really done much tuning beyond that. I do get some stringing but not too much. On the Snapmaker U1 I have it a hair faster. No real problems printing, but the Snapmaker's tuned pretty well out of the box. Have you done PA, volumetric flow tests, retraction, etc? I don't do anything temperature-wise much beyond whatever the Orca defaults for "generic petg" call for, although I think my bed's close to 80C. Oh, and I mostly print petg on a glue-coated smooth PEI plate because getting it off the textured PEI can be really annoying unless the print's relatively large so I can get a good plate flex when trying to take it off.
 
It can print fast, but did you run any strength tests on your prints?
 
It can print fast, but did you run any strength tests on your prints?
Like what?

I printed a few grocery store bag hooks so you can carry more of them in one trip. They work fine.
 
For PETG, I'm talking about long term stress on a part that needs to pinch or expand to conform to a shape over a long period of time. Like the locking tabs on a Raspi 4B case can opened and closed repeatedly without breaking off.
These were printed horizontally, so the force is being applied directly against the z axis layer line where the tabs lock in with the bottom case cover, so printing PETG at the recommended 80mm/s max speed should ensure you have the best layer adhesion for long term reliability. I tried printing this case in PLA and those tabs will snap right off, or warp over time, so if you open the case a year later, it might not have the same locking tension with PLA. There are no fillets at the tab's bottom edges either, which the original designers should have implemented.

I printed these cases over a year ago in PETG at 80mm/s, and the locking tabs still have not lost any tension nor have cracked and broken off. If I printed these at a much faster speed, those tabs would probably snap after some time.
I'm opening and closing an empty Raspi 4B case to show that the back of the tabs are not being supported by the Raspi PCB.





And I even tested PETG outdoors for one year, I needed something that was springy, but could pinch and hold itself in place. Unfortunately my design needs to be changed a little bit, as even PETG will warp under heavy constant prying force and factor in direct sunlight exposure everyday. But PLA would probably snap right off much sooner. However, this is not a good test against the Z axis. Published it here: https://www.printables.com/model/1404705-security-camera-blocker-for-street-lights-sunlight
This part needs a slight redesign change and be printed with ASA, though.
1793793905737.png


And if you have those textured plates that have a pattern, its best to print the first layer very hot and very slow with a lower z offset to hide the first layer extrusion lines. Most people probably don't care about this much detail though.
This was PETG at 8mm/s, 92C bed and 260C extrusion, only on the first layer.
1793794824648.png


Some of my other models need to be flexible and not warp. Hopefully printing at the recommended speeds would improve the lifespan of the part.
This PETG print is also over a year old and has been holding a round cylinder shaped object.
1793795258371.png
 

Attachments

  • PXL_20261104_114139444~2.mp4
    4.9 MB
Last edited:
Like what?

I printed a few grocery store bag hooks so you can carry more of them in one trip. They work fine.
If your part isn't designed to flex or stay under constant tension 24/7, then printing PETG at a faster speed probably won't affect your use case.
 
Well, i will admit I'm pretty new to this and haven't gotten to designing long term functional parts yet, really. My most paisa print was the car door lock knob cap thing i think i showed a while ago.
 
In my experience it isn't noticeably different. I've got several structural items printed without any issue. Printing it super fast requires the nozzle be so hot because there's less time to transmit the heat so if it is moving fast enough the temperature shouldn't be meaningfully different. I think this would obviously fall apart a bit if you have short layer times with small movements that don't let the extruder speed up and thus the heat could be more of a problem but it hasn't come up yet for me other than aesthetically.
 

Attachments

  • PXL_20261104_141843965.jpg
    PXL_20261104_141843965.jpg
    404.9 KB · Views: 0
  • PXL_20261104_150344399.MACRO_FOCUS (1).jpg
    PXL_20261104_150344399.MACRO_FOCUS (1).jpg
    156 KB · Views: 0
Back
Top